Главная " Overmolding Services

Overmolding Services

Elite Mold Tech overmolds one material over another to make a single, bonded part, such as a soft TPE grip over a rigid plastic handle or a seal molded onto a housing. Overmolding removes glue, screws, and assembly steps, and gives your product better grip, sealing, and feel. Sealing features hold ±0.05 mm, so gaskets seal the first time.

How Overmolding Works

Overmolding is done in two stages. First, a rigid part called the substrate is molded. Then it goes into a second mold cavity, where a second material is molded over or around it. The two materials bond chemically, mechanically, or both, and leave the mold as one part.

Two-Shot (2K) Molding

Both materials are molded in one machine and one cycle. The mold rotates or shifts between shots. It suits high volumes and gives the most consistent bond.

Pick-and-Place Overmolding

The substrate is molded first, then placed into a second mold by hand or robot. It costs less to tool and suits lower volumes or large parts.

Overmolded Parts We Make

Эргономичные рукоятки

Soft-touch grips on tools, kitchenware, and personal care products.

Потребительские товары из разных материалов

Two-color housings, buttons, and wearables with soft and hard zones in one part.

Компоненты медицинского оборудования

Soft seals, grips, and over-molded housings in medical-grade materials.

Which Materials Bond Together

A strong overmold starts with a compatible material pair. If the chemistry does not bond well, the joint must rely on a mechanical interlock.

СубстратCommon OvermoldBond
PPTPE (SEBS-based)Good chemical bond
ABSBondable TPE grades, TPUGood chemical bond
ПКBondable TPE grades, TPUGood chemical bond
PC/ABSTPU, bondable TPEGood chemical bond
Нейлон (PA)Modified TPE for nylonFair; add mechanical interlocks
POM (ацеталь)Most TPEsPoor; design mechanical interlocks
МеталлTPE, TPU, rigid plasticsMechanical, see insert molding

Tell us both materials and the load on the joint, and we will confirm the pair before tooling.

Overmolding Tolerances and Specifications

ХарактеристикаВозможности
Maximum part sizeAbout 508 × 508 × 254 mm (20 × 20 × 10 in); larger parts reviewed per project
Срок выполнения заказа4 to 6 weeks for dual tooling and sampling; shorter for single-shot with pre-molded inserts
General tolerances±0.127 to ±0.25 mm (±0.005 to ±0.010 in)
Precision tolerances±0.05 mm (±0.002 in) on critical areas such as sealing features
Minimum feature sizeAbout 0.5 mm (0.020 in), for soft ribs and textured grips
Толщина стенкиSubstrate ≥ 1.0 mm; overmold layer ≥ 0.5 mm, kept uniform
Угол наклона1° to 2° on the substrate; 3° to 5° on soft overmold material

Design Rules for a Strong Overmold

Add mechanical interlocks: Holes, grooves, or undercuts in the substrate lock the overmold in place.

Keep the overmold layer even: Uniform thickness avoids sink and uneven bonding.

Design clean shut-offs: A sharp edge where the soft material stops prevents flash on the rigid part.

Use more draft on soft material: 3° to 5° helps TPE release without tearing.

Avoid thin overmold at edges: Thin TPE at edges peels first.

Our design engineering team checks these in the DFM review.

Overmolding Materials

GroupМатериалы
Thermoplastics (substrate)ABS, polycarbonate, nylon, acrylic, PVC, polypropylene, PETG, POM (acetal)
Elastomers (overmold)TPE, TPU
РезиныSilicone, EPDM, Buna-N
Термореактивные материалыUrethane, epoxy, phenolic
Soft-touch materialsRubber and soft-touch TPE grades

Finishes for Overmolded Parts

As-molded: The finish straight from the mold

Textured: Grip patterns and matte surfaces on soft zones

Polishing: Gloss on rigid areas

Painting and coating: Color and protective coats

Литье с накладкой против литья со вставками

Overmolding usually bonds plastic to plastic, often a soft layer over a rigid part. Insert molding molds plastic around a pre-made insert, most often a metal thread, pin, or contact. Many parts use both. Both are built on our plastic injection molding capability.

Overmolded Parts Gallery

See soft-touch handles, two-material housings, and medical components overmolded by Elite Mold Tech.

Request an Overmolding Quote

Send your 3D files for both shots, the material pair, and your annual volume, and we will reply with a tooling and part quote. Your files stay private under our IP protection policy.

Свяжитесь с нами

Воплощайте свои проекты в жизнь с Elite Mold Tech

Испытайте прецизионную обработку с ЧПУ с Elite Mold Tech. От сложных прототипов до крупномасштабного производства - мы готовы воплотить ваши идеи в реальность. Свяжитесь с нами сегодня, чтобы обсудить потребности вашего проекта!

Свяжитесь с нами!
Оперативный ответ гарантирован в течение 12 часов
🔐 Все загрузки безопасны и конфиденциальны

Часто задаваемые вопросы по овермолдингу

Overmolding molds a second material over a first molded part so they become one bonded piece. A common example is a soft TPE grip over a rigid plastic handle. It removes glue and assembly steps.

TPE and TPU are the most common overmold materials, molded over ABS, PC, PP, and nylon. Silicone and other rubbers are also used. The pair must bond chemically or be locked with a mechanical interlock.

Two-shot molding is a type of overmolding where both materials are molded in one machine cycle. Pick-and-place overmolding molds the substrate first, then moves it to a second mold. Two-shot suits high volumes, while pick-and-place suits lower volumes.

Dual tooling and sampling usually take 4 to 6 weeks. Single-shot overmolding over pre-molded parts can be faster.

Peeling usually comes from a poor material pair, thin overmold at the edges, or no mechanical interlock. We check bonding and interlock design in the DFM review.

General tolerances are ±0.127 to ±0.25 mm. Sealing features can hold ±0.05 mm with stable materials and tooling.