Elite Mold Tech overmolds one material over another to make a single, bonded part, such as a soft TPE grip over a rigid plastic handle or a seal molded onto a housing. Overmolding removes glue, screws, and assembly steps, and gives your product better grip, sealing, and feel. Sealing features hold ±0.05 mm, so gaskets seal the first time.
Overmolding is done in two stages. First, a rigid part called the substrate is molded. Then it goes into a second mold cavity, where a second material is molded over or around it. The two materials bond chemically, mechanically, or both, and leave the mold as one part.
Both materials are molded in one machine and one cycle. The mold rotates or shifts between shots. It suits high volumes and gives the most consistent bond.
The substrate is molded first, then placed into a second mold by hand or robot. It costs less to tool and suits lower volumes or large parts.
Soft-touch grips on tools, kitchenware, and personal care products.
Two-color housings, buttons, and wearables with soft and hard zones in one part.
Soft seals, grips, and over-molded housings in medical-grade materials.
A strong overmold starts with a compatible material pair. If the chemistry does not bond well, the joint must rely on a mechanical interlock.
| 기판 | Common Overmold | Bond |
|---|---|---|
| PP | TPE (SEBS-based) | Good chemical bond |
| ABS | Bondable TPE grades, TPU | Good chemical bond |
| PC | Bondable TPE grades, TPU | Good chemical bond |
| PC/ABS | TPU, bondable TPE | Good chemical bond |
| 나일론 (PA) | Modified TPE for nylon | Fair; add mechanical interlocks |
| POM (아세탈) | Most TPEs | Poor; design mechanical interlocks |
| 금속 | TPE, TPU, rigid plastics | Mechanical, see insert molding |
Tell us both materials and the load on the joint, and we will confirm the pair before tooling.
| 기능 | 기능 |
|---|---|
| Maximum part size | About 508 × 508 × 254 mm (20 × 20 × 10 in); larger parts reviewed per project |
| 리드 타임 | 4 to 6 weeks for dual tooling and sampling; shorter for single-shot with pre-molded inserts |
| General tolerances | ±0.127 to ±0.25 mm (±0.005 to ±0.010 in) |
| Precision tolerances | ±0.05 mm (±0.002 in) on critical areas such as sealing features |
| Minimum feature size | About 0.5 mm (0.020 in), for soft ribs and textured grips |
| 벽 두께 | Substrate ≥ 1.0 mm; overmold layer ≥ 0.5 mm, kept uniform |
| 초안 각도 | 1° to 2° on the substrate; 3° to 5° on soft overmold material |
Add mechanical interlocks: Holes, grooves, or undercuts in the substrate lock the overmold in place.
Keep the overmold layer even: Uniform thickness avoids sink and uneven bonding.
Design clean shut-offs: A sharp edge where the soft material stops prevents flash on the rigid part.
Use more draft on soft material: 3° to 5° helps TPE release without tearing.
Avoid thin overmold at edges: Thin TPE at edges peels first.
Our design engineering team checks these in the DFM review.
| Group | 자료 |
|---|---|
| Thermoplastics (substrate) | ABS, polycarbonate, nylon, acrylic, PVC, polypropylene, PETG, POM (acetal) |
| Elastomers (overmold) | TPE, TPU |
| 고무 | Silicone, EPDM, Buna-N |
| 열경화성 | Urethane, epoxy, phenolic |
| Soft-touch materials | Rubber and soft-touch TPE grades |
As-molded: The finish straight from the mold
Textured: Grip patterns and matte surfaces on soft zones
Polishing: Gloss on rigid areas
Painting and coating: Color and protective coats
Overmolding usually bonds plastic to plastic, often a soft layer over a rigid part. Insert molding molds plastic around a pre-made insert, most often a metal thread, pin, or contact. Many parts use both. Both are built on our plastic injection molding capability.
See soft-touch handles, two-material housings, and medical components overmolded by Elite Mold Tech.
Send your 3D files for both shots, the material pair, and your annual volume, and we will reply with a tooling and part quote. Your files stay private under our IP protection policy.
엘리트 몰드 테크의 정밀 CNC 가공을 경험해 보세요. 복잡한 프로토타입부터 대규모 생산까지, 당사는 고객의 아이디어를 현실화할 준비가 되어 있습니다. 지금 바로 문의하여 프로젝트에 필요한 사항을 논의하세요!
Overmolding molds a second material over a first molded part so they become one bonded piece. A common example is a soft TPE grip over a rigid plastic handle. It removes glue and assembly steps.
TPE and TPU are the most common overmold materials, molded over ABS, PC, PP, and nylon. Silicone and other rubbers are also used. The pair must bond chemically or be locked with a mechanical interlock.
Two-shot molding is a type of overmolding where both materials are molded in one machine cycle. Pick-and-place overmolding molds the substrate first, then moves it to a second mold. Two-shot suits high volumes, while pick-and-place suits lower volumes.
Dual tooling and sampling usually take 4 to 6 weeks. Single-shot overmolding over pre-molded parts can be faster.
Peeling usually comes from a poor material pair, thin overmold at the edges, or no mechanical interlock. We check bonding and interlock design in the DFM review.
General tolerances are ±0.127 to ±0.25 mm. Sealing features can hold ±0.05 mm with stable materials and tooling.