| Property | Value |
|---|---|
| Mechanical Properties | |
| Ultimate tensile strength | 310 – 350 MPa |
| Yield strength | 220 – 240 MPa |
| Young’s modulus (modulus of elasticity) | 103 – 105 GPa |
| Elongation at break | 28 – 32 % |
| Hardness | 120 HB |
| Physical Properties | |
| Corrosion resistance | Excellent |
| Magnetism | Non-magnetic |
| Weldability | High |
| Thermal Properties | |
| Maximum service temperature | 320 – 400 °C |
| Thermal expansion coefficient | 8.35 – 8.6 × 10-6/ºC |
| Thermal conductivity | 16 – 21 W/(m⋅°C) |
| Electrical Properties | |
| Electrical resistivity | 42 – 45 μΩ*cm |
| Post Treatments | |
| Post-Processing | Cold & hot working, annealing. Not hardenable by heat treatment. |
| Anodizing compatibility | Suitable |
| Common Applications | |
| Airframe components | Cryogenic vessels |
| Heat exchangers | CPI equipment |
| Condenser tubing | Pickling baskets |