| Property | Value |
|---|---|
| Mechanical Properties | |
| Ultimate tensile strength | 620 – 700 MPa |
| Yield strength | 425 – 500 MPa |
| Young’s modulus (modulus of elasticity) | 195 – 205 GPa |
| Elongation at break | 14 – 28 % |
| Physical Properties | |
| Corrosion resistance | Excellent |
| Magnetism | Magnetic |
| UV resistance | Excellent |
| Weldability | Good |
| Thermal Properties | |
| Maximum service temperature | 335 – 365 °C |
| Thermal expansion coefficient | 13.5 – 18.2 × 10-6/ºC |
| Thermal conductivity | 14.4 – 15.6 W/(m⋅°C) |
| Electrical Properties | |
| Electrical resistivity | 78.4 – 81.6 μΩ*cm |
| Post Treatments | |
| Post-Processing | Hardening |
| Anodizing compatibility | Not suitable |
| Common Applications | |
| Environments containing chlorides and hydrogen sulphide | Flue gas filters |
| Chemical tanks | Heat exchangers |
| Acetic acid distillation components | |